Carbodiimide-uretonimine modified 4,4'-MDI diluted with 4,4'-MDI for the synthesis of polyurethane prepolymers
Features
-
NCO :
31 - 33 m/m%
-
Viscosity @25°C :
5 - 30 mPa.s
-
Functionality :
2.0
-
INDUSTRIAL SEGMENTConstruction
Applications
- CASE: Coatings, Adhesives